  • text
  • asciidoc
  • rtf
Study of thermal annealing on gallium oxide heteroepitaxial layers grown on SiC for vertical Schottky barrier diodes applications
Natl Yang Ming Chiao Tung Univ, Taiwan.
Natl Yang Ming Chiao Tung Univ, Taiwan.
Natl Yang Ming Chiao Tung Univ, Taiwan.
Linköpings universitet, Institutionen för fysik, kemi och biologi, Tunnfilmsfysik. Linköpings universitet, Tekniska fakulteten.ORCID-id: 0000-0001-7192-0670
Visa övriga samt affilieringar
2024 (Engelska)Ingår i: Applied Surface Science Advances, E-ISSN 2666-5239, Vol. 24, artikel-id 100661Artikel i tidskrift (Refereegranskat) Published
Abstract [en]

This study successfully grew (3-Ga2O3 epitaxial films on silicon carbide substrates by metalorganic chemical vapor deposition and fabricated vertical Schottky barrier diodes (SBDs), which were annealed in a high temperature furnace. The high surface roughness and oxygen vacancies of the unannealed device caused a large leakage current, thus three different annealing durations were used to repair the surface oxygen vacancies in an O2: N2=1:4 gas environment. The results showed that a 5-minute thermal annealing process was the most effective in repairing surface oxygen vacancies. According to the X-ray photoelectron spectroscopy spectra of the O 1 s core levels in Ga2O3 epilayers, the proportion of oxygen vacancies decreased from 56.56 % to 49.71 %. Additionally, the leakage current density was decreased from 10-3 to 10-5 A/cm2 and the surface roughness decreases to 32.6 nm due to stress release. Furthermore, the barrier heights (phi b) of the SBDs without annealing, and after annealed for 5, 20, and 40 min were measured at 0.911, 1.229, 1.090, and 1.115 eV, respectively. It was observed that the SBD fabricated on the epilayer annealed for 5 min exhibited the lowest leakage current (approximately 2 x 10-5 A/cm2) and the highest breakdown voltage, measuring around 132 V.

Ort, förlag, år, upplaga, sidor
ELSEVIER , 2024. Vol. 24, artikel-id 100661
Nyckelord [en]
Silicon carbide substrates; Metalorganic chemical vapor deposition; Gallium oxide (Ga 2 O 3 ); Annealing; Schottky barrier diode (SBD); Oxide vacancy
Nationell ämneskategori
Den kondenserade materiens fysik
Identifikatorer
URN: urn:nbn:se:liu:diva-210140DOI: 10.1016/j.apsadv.2024.100661ISI: 001360588900001OAI: oai:DiVA.org:liu-210140DiVA, id: diva2:1917578
Anmärkning

Funding Agencies|National Science and Technology Council (Taiwan, R.O.C.) [112-2622-E-A49-011, 112-2221-E-A49-069-MY3, 112-2622-8-A49-013-SB, 111-2923-E-A49-003-MY3, 110-2222-E-009-006-MY3, 113-2923-E-A49-010-MY2, 113-2811-E-A49-513-MY3]

Tillgänglig från: 2024-12-03 Skapad: 2024-12-03 Senast uppdaterad: 2024-12-03

Open Access i DiVA

Fulltext saknas i DiVA

Övriga länkar

Förlagets fulltext

Sök vidare i DiVA

Av författaren/redaktören
Hsiao, Ching-Lien
Av organisationen
TunnfilmsfysikTekniska fakulteten
I samma tidskrift
Applied Surface Science Advances
Den kondenserade materiens fysik

Sök vidare utanför DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetricpoäng

doi
urn-nbn
Totalt: 41 träffar
RefereraExporteraLänk till posten
Permanent länk

Direktlänk
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • oxford
  • Annat format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annat språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf