The very high cycle fatigue performance of four ductile cast irons, a solid solution strengthened ferritic, ferritic-pearlitic, and two austempered ductile cast irons, was investigated by ultrasonic fatigue testing under fully reversed loading conditions. The step-stress fatigue testing method incorporating re-use of runouts was employed, with a 3x108$$ 3\times 1{0}<^>8 $$ cycles to failure runout criteria. The guarantee of failed specimens enables extensive fractography and characterization of fatigue-initiating defects, facilitating extreme value analysis of defect distributions. Furthermore, the fatigue and defect data were used for evaluation of stress-cycle-defect relationships as well as fatigue strength distributions. The obtained relationships between applied stress and fatigue-initiating defect size were used to adjust the data with respect to a given defect size, to compare and evaluate fatigue-initiating defect size equivalent fatigue strength distributions, emphasizing the role of the different matrix microstructures.
Funding Agencies|Swedish Energy Agency; Formas; Vinnova [2021-04007]; Epiroc Rock Drills AB; Vinnova [2021-04007] Funding Source: Vinnova