Replenishing the oxidation-induced Al-depletion in Cr2AlC MAX phase coatings
Rhein Westfal TH Aachen, Germany; Univ Bordeaux, France.
Rhein Westfal TH Aachen, Germany.
Rhein Westfal TH Aachen, Germany.
Linköping University, Department of Physics, Chemistry and Biology, Thin Film Physics. Linköping University, Faculty of Science & Engineering. Uppsala Univ, Sweden.ORCID iD: 0000-0003-1785-0864
Show others and affiliations
2026 (English)In: Materials & design, ISSN 0264-1275, E-ISSN 1873-4197, Vol. 267, article id 116316Article in journal (Refereed) Published
Abstract [en]

Cr2AlC MAX phase coatings are known to form a protective alumina scale upon high temperature oxidation. Scale formation causes Al depletion, which results in the formation of Cr-carbides and pores that, in turn, cause coating failure. Here, we show that the oxidation-driven Al depletion of the coating is prevented by Al-replenishment using an Al-reservoir (Al-containing substrate), thereby extending the coating lifetime. Cr2AlC substrates with coarse and fine grain distributions were produced by spark plasma sintering and coated with Cr2AlC by magnetron sputtering. Upon oxidation at 1100 degrees C the Cr2AlC coatings, deposited onto a coarse-grained reservoir and onto MgO without an Al-reservoir, showed no significant change in Al content of the coating post-oxidation, and hence no evidence for Al-replenishment from the substrate. However, in the case of a Cr2AlC coating deposited onto a fine-grained substrate, the Al content of the coating post-oxidation remained close to the initial concentration (similar to 23 at.%). This replenishment is rationalized by the presence of more grain boundaries in the fine-grained substrate, versus the coarse-grained one, enabling sufficient Al diffusion across the substrate/coating interface to offset the Al losses to the scale.

Place, publisher, year, edition, pages
ELSEVIER SCI LTD , 2026. Vol. 267, article id 116316
Keywords [en]
Nanolaminates; MAX phases; Oxidation; Al-reservoir; Diffusion; Interface
National Category
Manufacturing, Surface and Joining Technology
Identifiers
URN: urn:nbn:se:liu:diva-225411DOI: 10.1016/j.matdes.2026.116316ISI: 001792866100001OAI: oai:DiVA.org:liu-225411DiVA, id: diva2:2076764
Note

Funding Agencies|European Union [892501]; Knut and Alice Wallenberg foundation [KAW-2020.0196]; Swedish Research Council (VR) [2021-03826]

Available from: 2026-06-22 Created: 2026-06-22 Last updated: 2026-08-21

Open Access in DiVA

fulltext(5631 kB)7 downloads
File information
File name FULLTEXT01.pdfFile size 5631 kBChecksum SHA-512
4eebbf7bb532be9070676b6aa37f0439e193c8d4d70f0c5a56d6791851612c3d9426986456f6310bf60e38946190c8cc1013b783a7d2579dd67a4a3fc87e141f
Type fulltextMimetype application/pdf

Other links

Publisher's full text

Search in DiVA

By author/editor
Eklund, Per
By organisation
Thin Film PhysicsFaculty of Science & Engineering
In the same journal
Materials & design
Manufacturing, Surface and Joining Technology

Search outside of DiVA

GoogleGoogle Scholar
Total: 7 downloads
The number of downloads is the sum of all downloads of full texts. It may include eg previous versions that are now no longer available

doi
urn-nbn

Altmetric score

doi
urn-nbn
Total: 30 hits
CiteExportLink to record
Permanent link

Direct link
Cite
Citation style
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • oxford
  • Other style
More styles
Language
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Other locale
More languages
Output format
  • html
  • text
  • asciidoc
  • rtf