High quality epilayers with a minimum of microstructural features can act as test beds to elucidate intrinsic materials properties and improve the understanding of more complex materials. We report on the growth of epitaxial Ti1-xAlxNy thin films with low aluminium content (x = 0-0.4) on MgO (001) substrates using reactive magnetron co-sputtering from a pure Ti and a compound Ti0.75Al0.25 target. The films are fully strained and display a pronounced (001) orientation with low mosaicity and high lateral coherence. The hardness increases up to 29 GPa because of solid-solution hardening and coherency strains associated with early-stage spinodal decomposition, despite an increase in tensile residual stress with Al content. Electrical resistivity increases as the charge carrier concentration decreases with Al content, because enhanced solute scattering and progressive depletion of the metallic Ti-3d-N-2p hybridized conduction band. Al substitution for Ti introduces lattice distortions that increase disorder, reflected by a decreasing Ioffe-Regel parameter (kFl) with Al content. Mobility shows a non-monotonic trend, first decreasing and then increasing with Al content. The changes in electrical resistivity, carrier density, mobility and Ioffe-Regel parameter imply a shift from metallic to increasingly localized electronic transport with increasing Al incorporation.
Funding Agencies|VINNOVA, Sweden; Competence Centre FunMat-II [2022-03071]; Swedish Research Council, Sweden; VRRFI [2019_00191]